Good handle feeling hydrophilic Silicone Oil RH-NB-8098-6 is modified quaternary ammonium multi-copolymerized polymer polysiloxane.
1.Endow fabric excellent hydrophilic after using, can comparable the hydrophilic with traditional polyether silicone oil, improving the quality of textile, endowing the clothes excellent wear comfortable.
2.Endow fabric amino silicone oil's softness, smoothness,elastic,strong cotton simple feeling.
3..No yellowing change, less discolour, no effect to color light.
4.High shear resistant,no roller-sticky,excellent stability.
5.If found the color is not right after dying, no need to remove the softener when re-dying, won't effect the dying, color deep, pure and bright.
6.It can be used together with cationic/non-ionic softener to increase the whole property largely.
7.High performance to price rate.
Appearance:little yellow transparent liquid
Ionicity: weak cationic
Solid content: 85-87%
Apply to the soft hydrophilic finishing for the fabric which mainly containing cellulose fiber or protein fiber.
Recommend to dilute 20% emulsion to use.
(1) Dipping Process: RH-NB-8098-6 diluted emulsion 2-6%(o.w.f)
(2) Padding Process: RH-NB-8098-6diluted emulsion 10-40g/L
100kg or 190kg plastic barrel.
Store in cool and ventilated warehouse. 6 months of storage period.
RH-NB-8098-6: 200kg
Emulsifier: 40kg
Acid water: 5kg Glacial acetic acid+5kg water
Water: 360kg
Dilute process:
1. Add RH-NB-8098-6 and emulsifier to reactor, start stirring for 5-10 minutes;
2. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;
3. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;
4. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;
5. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;
6. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;
7. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;
8. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;
9. Add 30kg water to stir for 5 minutes; add 1 kg acid water to stir for 5-10 minutes;
10. Slowly add rest water while stirring, add rest acid water, stir evenly for 5-10 minutes, add glacial acetic acid to adjust PH value to 5-6
Notice: Must use high speed machine, last time can add water slowly.
Emulsifier: XL40:XL90=1:1